The reduction in strength after 28 and 90 days by K 2 O contents up to 1.5 per cent can be offset by lowering the alumina ratio where there is an optimum degree of sulfatisation, but the reduction in strength caused by Na 2 O contents up to 1.5 per cent is only partly compensated.